Sealing and glazing

Boat Window and Glass Bonding, Portlight Sealing

We remove leaking boat windows, glazing and portlight seams, prepare the surfaces and re-bond them with polyurethane adhesive to the product data sheet. We find the source of the leak first, then apply a lasting fix.

  • On-site survey
  • Written quotation
  • Documented handover
  • 7 min read
  • Updated:
  • SourceThe real origin of the leak is found first
  • PUFlexible polyurethane bonding layer
  • Zero siliconeSilicone residue fully removed
  • WrittenItemised scope and quotation

Windows and portlights are the most common leak points on a boat. Boat windows are usually bonded into a frame or sealed to the frame with a gasket. Bonding is a structural process that ties the glass to the hull and also provides the seal. Poor surface preparation or the wrong product leads to leaks, timber rot and, over the years, windows working loose. That is why we carry out bonding and sealing with the right surface preparation, the right product and the right sequence.

In short:

  • Bonding is won through surface preparation: a clean, dry surface primed to suit the product is essential.
  • Polyurethane (PU) adhesive stays flexible and absorbs vibration and expansion.
  • PU does not bond reliably to a silicone-contaminated surface; silicone residue must be removed completely.
  • If water getting in around the frame goes unnoticed, the timber and the interior get damaged.

Where we work on windows, glazing and seams#

Window, glass and seam areas on a boatTap a number or the list to see what we do in each area.
Side view diagram of a yacht; the areas covered by this service are marked with numbers. Waterline 1 2 3 4

Tap a number or an area in the list.

Our window and glass bonding scope
JobWhat we doGuide
Leak detectionInterior traces, exterior check and zone-by-zone water testLeak detection
Glass / acrylic removalMechanical removal with cutting wire or knife, without damaging the frameSikaflex applications
Re-bondingCleaning, primer/activator, continuous PU bead, support and curingSikaflex applications
Portlight and hatch seamsOld seam removal, primer, void-free new seam, seal checkLeak detection
Timber damageRepair of interior damage caused by water ingressCockpit and exterior timber

Window bonding cross-section: what does the glass sit on?#

Window bonding cross-section
  1. 1
    Glass / acrylicWindow glass or acrylic sheet
  2. 2
    PU adhesive layerFlexible, void-free bond of sufficient thickness
  3. 3
    Primer / activatorAdhesion preparation matched to product and surface
  4. 4
    Substrate: frame or hull surfacePainted or laminate; clean, dry, grease-free

The adhesive layer must be thick enough and void-free; the edge seam provides the seal.

As the cross-section shows, the glass does not sit directly on the hull but on a flexible bonding layer. This layer absorbs the different rates at which the glass and the hull expand. Thickness and the edge seam are set to the manufacturer's recommendation.

Why do boat windows leak?#

  • A seam around the frame that has dried out, cracked or separated
  • Areas where surface preparation was incomplete and the bond has lifted
  • Old repairs made with silicone
  • Glass or frame moving under impact and stress
  • Water entering through bolt and screw holes
  • An old gasket that has hardened and stopped doing its job

Step by step: boat window and glass bonding#

Window bonding workflow
  1. Removal: old glass
  2. Cleaning: no silicone trace
  3. Primer: activator
  4. Bond: adhesive bead
  5. Support: hold in place
  6. Cure: wait

The bonding system and times vary by product.

  1. Removal

    The old glass and adhesive are removed mechanically (cutting wire or knife), taking care not to damage the frame and the surrounding surface.

  2. Cleaning off the old product

    Residual adhesive is scraped back to a thin layer; every trace of silicone is removed.

  3. Surface preparation

    The surface is wiped with solvent. Adhesion of the painted surface is checked. The surface is sanded if needed.

  4. Activator and primer

    An activator or primer suited to the product and surface is applied and the waiting time observed.

  5. Applying the adhesive

    The adhesive is applied as a continuous bead with no gaps.

  6. Setting the glass

    The glass is placed and pressed in gently; the bond thickness is set. It is held with supports and tape.

  7. Curing and clean-up

    Excess product is cleaned off and the tapes removed. No load is put on the glass until curing is complete.

Hatch and portlight perimeter seams#

The seams around hatches and portlights seal the joint with the hull or deck. Flexibility and adhesion matter in these seams. The seam is laid as a bead surrounding the frame; before working under the frame, the old product is removed and the surface cleaned.

The portlight seal must also be checked separately; a hardened or crushed gasket lets water through. Renewing the seam and replacing the gasket together reduces the risk of leaks. For more, see our Sikaflex applications and leak detection guides.

Common mistakes in glass bonding#

Correct practice
  • Applying PU to a surface fully cleaned of silicone
  • Applying the right activator and primer with its waiting time
  • Laying a continuous, void-free adhesive bead
  • Keeping load off the glass until curing is complete
  • Finding the real source of the leak first
  • Renewing the old gasket together with the seam
Common mistakes
  • Applying PU to a surface with silicone traces
  • Skipping the activator and primer
  • Laying an insufficient or broken adhesive bead
  • Loading the glass before curing is complete
  • Only repairing the visible seam without finding the real source of the leak
  • Not replacing the old gasket

Boat window and glass bonding FAQ#

How long does a bonded window take to cure?

A skin forms on the surface within hours, while full cure takes days depending on thickness, temperature and humidity. The times in the product data sheet apply; no load is put on the window before it has cured.

Can windows be bonded with silicone?

It is generally not recommended on boats. Silicone has weak adhesive strength, and the residue left on the surface spoils any later PU application.

What happens if the glass cracks?

The glass is replaced. The frame and bonding surface are cleaned of old products, and the new glass is bonded using the same method.

Does the whole glass have to come out if a window leaks?

Not always. If the leak is only coming from the perimeter seam, the seam can be renewed. If the bond has lifted or the frame is loose, the glass is removed.

How are portlight and hatch seams renewed?

The old seam is removed mechanically, the surface cleaned, the required primer applied and the new seam filled without voids. The gaskets are checked separately.

What determines the cost of boat window bonding?

The number and size of windows, whether the glass has to come out, the condition of old product and silicone residue, any damage to surrounding timber and the product system used. A firm figure is given in writing, itemised, after the survey.

How long does window bonding take?

It depends on the number of windows, how difficult removal and cleaning are, the product's waiting and curing times and the weather. An estimated schedule is given in writing after the survey.

Related searches

People looking for this service also search for

All of the topics below are covered by this service and delivered by the same team under one plan.

  • boat window bonding
  • boat glass bonding
  • yacht window bonding
  • yacht glass bonding
  • boat window replacement
  • yacht window replacement
  • boat glass replacement
  • boat window sealing
  • leaking boat window
  • boat window leak repair
  • yacht window leak
  • portlight sealing
  • portlight rebedding
  • portlight seal replacement
  • porthole leak repair
  • hatch rebedding
  • hatch seal repair
  • boat hatch leaking
  • acrylic window replacement boat
  • perspex boat window
  • plexiglass boat window replacement
  • polyurethane window adhesive
  • PU adhesive for boats
  • Sikaflex window bonding
  • Sikaflex glass bonding
  • marine window sealant
  • boat window caulking
  • how to bond boat windows
  • how to remove boat windows
  • how to fix a leaking boat window
  • boat window bonding cost
  • yacht window replacement price
  • boat window bonding service
  • yacht glazing service
  • motor yacht window replacement
  • sailboat window rebedding
  • gulet window sealing
  • catamaran window replacement
  • silicone on boat windows
  • glass primer activator
  • cabin window bonding

On-site survey

Let us inspect your yacht together

We assess the condition on site and provide a written plan and quotation with scope, timing and price.