Hull, gelcoat and fibreglass repair

Fibreglass (GRP) Boat Repair: Cracks, Holes and Laminate Repair

We diagnose cracks, holes and impact damage on your fibreglass (GRP) boat by depth, restore structural thickness with scarf grinding and layer-by-layer lamination, and finish with gelcoat or paint.

  • On-site survey
  • Written quotation
  • Documented handover
  • 7 min read
  • Updated:
  • DiagnosisDamage depth and moisture first
  • 12:1Common scarf grinding ratio
  • Layer by layerStructural thickness rebuilt in plies
  • In writingRepair method presented in writing

Polyester (GRP, fibreglass) boats are built from glass-fibre-reinforced resin. The success of a damage repair depends on correctly understanding the depth of the damage, preparing the surface properly and restoring structural thickness layer by layer. Fibreglass boat damage such as cracks, holes and impact damage must be diagnosed correctly, and it must be established from the outset which repair is structural and which is cosmetic. A survey is essential for structural damage.

In short:

  • First, the depth of the damage is determined: gelcoat, laminate or sandwich core.
  • In a structural repair the damaged area is scarf ground and new plies are laid up layer by layer.
  • Epoxy bonds to polyester; the reverse is not reliable. If you repair with polyester, use the same type of resin.
  • Resin and hardener must be mixed at the correct ratio; temperature and humidity must stay within the product's limits.

Fibreglass boat damage types and general approach#

Where we work during a fibreglass repairTap a number or the list to see what we do in each area.
Side view diagram of a yacht; the areas covered by this service are marked with numbers. Waterline 1 2 3 4 5

Tap a number or an area in the list.

Fibreglass damage types
DamageAppearanceGeneral approach
Surface scratchStays in the gelcoatGround, filled with gelcoat paste, polished
Spider crackWeb-like cracks in the gelcoatOpened in a V and filled; the cause is investigated (a flexing area?)
Laminate crack / holeGlass fibre visible, fracturedScarf ground, new plies laid up, finished with gelcoat or paint
Sandwich core damageBalsa / foam wet, sounds differentWet core removed and dried; core and skins rebuilt

Materials and resin selection for fibreglass repair#

  • Polyester resin: Economical and compatible with the original material; it releases styrene while curing, so good ventilation is required.
  • Vinylester: Better water resistance than polyester; an intermediate solution.
  • Epoxy: Strong adhesion, low shrinkage and high water resistance; it is expensive.
  • Glass fibre: Chopped strand mat (CSM) for bulk and the first plies, woven roving for strength, biaxial for multidirectional loads.
  • Hardener: With polyester usually a few per cent by weight; the manufacturer's ratio must be followed.
Cross-section of a fibreglass repair area
  1. 1
    Gelcoat or paintFinish coat; colour and surface protection
  2. 2
    Fairing fillerSmoothing the ground surface
  3. 3
    Woven / biaxial pliesStrength and multidirectional loads; plies cut from small to large
  4. 4
    Chopped strand mat (CSM) first plyFirst ply bonding to the old laminate, and bulk
  5. 5
    Substrate: scarf-ground laminateLoose material removed, clean and dry; edges usually at 12:1 or a gentler taper

Number of plies, fibre type and resin are chosen according to the depth of the damage and the technical data sheet of the product used.

Fibreglass boat repair step by step#

General workflow of a fibreglass repair
  1. Diagnose: depth and moisture
  2. Grind: scarf taper
  3. Laminate: ply by ply
  4. Cure: temperature and time
  5. Fair: sand and smooth
  6. Finish: gelcoat / paint

Each ply is applied before the previous one has fully cured, or after the surface has been prepared.

  1. Clean and measure the damage

    Loose and crushed material is removed. The depth of the damage, the fracture boundary and moisture are measured.

  2. Scarf grinding

    The edges are usually ground to a 12:1 or gentler taper. This lets the new plies bond to the old laminate over a large surface.

  3. Surface cleaning

    Dust is removed and the surface is wiped with solvent. No grease or wax may remain.

  4. Cutting the fibre

    Plies are cut from small to large relative to the repair area.

  5. Resin and lamination

    The resin is mixed; the first ply of mat and the following plies are wetted out in sequence and rolled to remove air.

  6. Curing

    The product's temperature and time conditions are respected for full cure.

  7. Fairing and finishing

    The surface is sanded, faired with filler and sealed with gelcoat or paint.

Application conditions and safety in fibreglass repair#

Checks before lamination0/5
  • Temperature: Most resins cure properly at about 15–25 °C. Curing slows down in the cold and speeds up a lot in the heat.
  • Moisture: The surface and the fibre must be dry.
  • Mixing: Too little hardener leads to incomplete cure; too much makes the resin brittle.
  • Protection: Respirator (organic vapour), gloves, goggles and long-sleeved workwear.
  • Ventilation: Work in an open or ventilated area because of styrene vapours.

Common mistakes in fibreglass repair#

Correct practice
  • Grinding the edges to a long enough taper (usually 12:1 or gentler)
  • Drying the laminate and measuring moisture before the repair
  • Applying resin and fibre in thin plies, layer by layer
  • Epoxy over epoxy; the same type of resin for a polyester repair
  • Finding and eliminating the cause of the damage first
Common mistake
  • Keeping the scarf taper short. This creates a limited bonding surface.
  • Repairing damp laminate.
  • Applying too much resin and fibre in one go. This causes overheating and cracking.
  • Applying polyester over epoxy.
  • Only repairing the appearance without eliminating the cause of the damage.

Detailed guides on this topic#

Separate step-by-step, illustrated guides prepared for each work item:

  • Moisture measurement, drying and survey: How is moisture measured on a boat? Measuring points, types of moisture meter, drying follow-up, osmosis and sandwich deck moisture, post-damage survey and reporting.

Fibreglass boat repair FAQ#

Is a fibreglass repair durable?

A repair made with proper preparation, enough fibre and the right resin can be as durable as the original laminate. However, cosmetic appearance and structural strength are different matters.

Should epoxy or polyester be used?

Polyester is economical and compatible with the original material. Epoxy gives higher adhesion and water resistance. Epoxy bonds to polyester, but polyester does not bond reliably to cured epoxy.

Can a boat that has taken on water be repaired?

The moisture must first be removed completely. A repair applied to wet laminate will not bond, and the problem will grow.

Can a holed boat be repaired at sea?

In an emergency, temporary waterproof tapes, putty and plugs can be used; the permanent repair must be done ashore.

Will there be a colour difference at the repair?

Paint or gelcoat colour matching is required separately. For details, see our gelcoat repair page.

What determines the price of a fibreglass repair?

The type and depth of the damage, the size of the area, whether the sandwich core is affected, moisture in the laminate, the resin and fibre chosen, and whether the finish is gelcoat or paint determine the price. A firm figure is given in writing after an on-site inspection.

How long does a fibreglass repair take?

It depends on the extent of the damage, the number of plies needed, the resin's curing conditions and whether the laminate is dry. Damp laminate must be dried first. The schedule is confirmed in writing after an on-site inspection.

Related searches

People looking for this service also search for

All of the topics below are covered by this service and delivered by the same team under one plan.

  • fibreglass boat repair
  • fiberglass boat repair
  • GRP repair
  • GRP boat repair
  • polyester boat repair
  • boat hull repair
  • fibreglass hull repair
  • laminate repair
  • boat laminate repair
  • fiberglass crack repair
  • boat hole repair
  • impact damage repair boat
  • gelcoat crack repair
  • spider crack repair
  • stress crack repair boat
  • sandwich core repair
  • balsa core replacement
  • wet balsa core repair
  • foam core repair
  • scarf grinding
  • scarf repair 12:1
  • layer by layer lamination
  • chopped strand mat
  • woven roving
  • biaxial cloth
  • polyester resin
  • vinylester resin
  • epoxy resin boat repair
  • epoxy or polyester for boat repair
  • does epoxy stick to polyester
  • how to repair a fibreglass boat
  • how long does fibreglass repair take
  • fibreglass repair cost
  • boat hull repair price
  • repairing a hole in a boat hull
  • motor yacht hull repair
  • sailboat fibreglass repair
  • gulet hull repair
  • catamaran hull repair
  • fibreglass repair service

On-site survey

Let us inspect your yacht together

We assess the condition on site and provide a written plan and quotation with scope, timing and price.