InternationalFiller and fairing

Interfill 833: how is the general-purpose filler applied?

Two-pack general-purpose filler: 1:1 volume mix, applied with knife or trowel, 30 minutes pot life at 23 °C and sanding after 6 hours.

  • 4 min read
  • Updated:

Interfill 833 is a two-pack filler used for surface correction and fairing. It is suitable for correcting surface roughness and pits.

Interfill 833 is applied according to coat thickness. The technical data sheet clearly states temperature limits and recoat times.

Interfill 833 position in the system
Topcoat after sanding.

What does Interfill 833 do and where does it sit in the paint system?#

Interfill 833 is a filler coat used to level the surface and fair it.

Which surfaces and where is it used?#

  • Surface correction and fairing
  • Filler under Interprime 820 or Microsurfacer
  • Correction on sanded surface

Surface preparation: the stage that decides the outcome#

Surface must be clean, dry and grease-free. A knife or trowel is used for an even surface.

Pre-application checklist0/4

Mix ratio, induction and pot life#

Base and hardener (YAA815) are mixed at 1 : 1 by volume. No thinning is done.

YTA061 (No.7) is used for cleaning; before gelling.

Interfill 833 mixing and cleaning
ValueDescription
Mix1 : 1 (volume)
ReductionNone
CleaningYTA061 (No.7)
Pot life (23 °C)30 minutes

Application: step by step#

Applied with a knife or trowel. Coat thickness is variable; around 133 µm dry film is targeted.

Interfill 833 application
Short pot life.
  1. Mix

    1 : 1 by volume.

  2. Apply

    Knife or trowel.

  3. Cure

    Sand after 6 hours at 23 °C.

  4. Recoat

    Min 6 h.

  5. Sanding

    No topcoat without sanding.

Interfill 833 coat values
ParameterValue
Dry film / coatApproximately 133 µm
Sanding (23 °C)6 h
Recoat (min)6 h

Drying and recoat times#

Interfill 833 has a 30-minute pot life at 23 °C; sanding can be done after 6 hours.

Interfill 833 times
Pot life 30 minutes.
Interfill 833 times
Stage (23 °C)Time
Pot life30 min
Sanding6 h
Recoat (min)6 h

Application conditions: temperature, humidity and dew point#

Product applied at 10–25 °C; ambient 10–35 °C; surface 10–30 °C.

Interfill 833 application conditions
Temperature limits.

Tips from the professionals#

  • Apply within the pot life.
  • Do not apply a topcoat without sanding.
  • Keep the surface clean and dry.
  • Follow the temperature limits.

Common mistakes#

Correct practice
  • 1 : 1 volume mix
  • Application within pot life
  • Topcoat after sanding
  • Surface cleanliness
Common mistake
  • Application below 10 °C
  • Topcoat without sanding
  • Application over single-pack paint
  • Reduction

Health and safety#

Frequently asked questions#

What is the Interfill 833 mix ratio?

1 : 1 by volume.

Which thinner is used with Interfill 833?

None; YTA061 (No.7) for cleaning.

What is the Interfill 833 pot life?

30 minutes at 23 °C.

When is Interfill 833 sanded?

After 6 hours at 23 °C.

_Source: International Yacht Paint (AkzoNobel) product technical data sheet (TDS) and product page (Interfill 833 product data sheet). The values on this page are compiled from the manufacturer's published documents and may change as the product develops. Before application, always check the product label, the current technical data sheet (TDS) and the safety data sheet (SDS)._

On-site survey

Right product, right application

We inspect your boat on site and recommend the suitable system in writing.