Seajet 015 Underwater Primer is an acrylic sealer and barrier coat.
Mixing, thinning, film thickness, drying times and application conditions are summarised from the manufacturer data sheet.
What is Seajet 015 Underwater Primer for and where is it used?#
- Primer under antifouling on GRP and wood
- Barrier coat over old antifouling
Surface preparation#
- Apply only to dry, damp-free surfaces.
- Roughen old antifouling with P100–120.
- Degrease and abrade GRP and wood, then wipe with SEAJET Thinner E.
Mixing and thinning#
It is a single-pack product with no mix ratio. Stir well before use.
Thinner: SEAJET THINNER A, ratio 15–25 % (by volume).
Application method and film thickness#
- Application methods: Airless spray, Brush, Roller.
- Wet film per coat: 100 µm
- Dry film per coat: 30 µm
- Number of coats: 1 coat over existing antifouling; 3 coats on bare GRP; 3–4 coats on wood
- Theoretical coverage: 10.0 m²/l
- Volume solids: 30 ±2 %
- Equipment: Graco 721/723 tip, 15.0–18.0 MPa
Drying and recoat times (20 °C)#
- Surface dry: 20 min
- Hard dry: 2 h
- Minimum recoat interval: 3 h
- Maximum recoat interval: no limit
Drying times increase with film thickness; make sure the film is fully dry before recoating.
Application conditions#
- Minimum temperature: Ambient and product 5 °C, substrate 7 °C
- Maximum temperature: 35 °C
- Maximum relative humidity: 85 %
- Do not apply in rain, fog, condensation or direct sun; make sure the surface is dry.
Compatible products and system#
- Subsequent coats: All SEAJET antifoulings
- Shelf life: minimum 3 years (20 °C)
Common mistakes#
- Applying without degreasing and abrading the surface
- Changing the mix ratio
- Missing the recoat window and painting without abrading
- Applying in damp or cold conditions
Health and safety#
The product is flammable; keep it away from sparks and open flames and do not smoke in the work area. Ventilate, and avoid skin contact and inhaling spray mist. In case of eye contact, rinse with plenty of water and seek medical advice. Do not pour waste into drains. VOC (theoretical): 614 g/l.
Frequently asked questions#
How many coats of Seajet 015 Underwater Primer are applied?
Value stated in the data sheet: 1 coat over existing antifouling; 3 coats on bare GRP; 3–4 coats on wood.
How long does Seajet 015 Underwater Primer take to dry at 20 °C?
Surface dry: 20 min; Hard dry: 2 h.
How is Seajet 015 Underwater Primer thinned?
Value stated in the data sheet: SEAJET THINNER A: 15–25 %.
_Source: Chugoku Paints B.V. Seajet technical data sheet (Seajet 015, 01-06-2022). The values on this page are compiled from the manufacturer’s published documents and may change as the product develops. Before application, always check the product label, the current technical data sheet (TDS) and the safety data sheet (SDS)._