Paint and Coatings

Why Does Orange Peel Occur in Paint?

When reflections look wavy on a glossy painted surface it is often orange peel. This article explains the defect’s causes, correction options and prevention, based on paint makers and general sources.

  • 8 min read
  • Updated:
  • Level: Technical guide

Short answer

Orange peel is a textured, bumpy look when the paint film fails to flow out and level. Sources list among causes high viscosity (thick paint), fast thinner or hardener, low atomisation pressure and a gun held too far, too much paint applied by roller and extreme heat or cold. Light cases can be corrected by wet sanding and polishing; deep orange peel needs sanding and a fresh coat. Prevention: thinning per the data sheet, correct setup and thin coats. This article is general information.

Key points

  • Orange peel is a textured surface from paint failing to flow out and level.
  • Causes: high viscosity, fast thinner or hardener, low pressure, far gun, too much paint by roller, extreme heat or cold.
  • For light cases wet sanding and polish may be enough; for deep cases sanding and recoat are needed.
  • When sanding there is a risk of going through the paint to the layer below; check film thickness.
  • Prevention: thinning per data sheet, correct gun or roller technique and suitable conditions.

1. What is orange peel?#

Orange peel is a wavy, textured look resembling orange skin that results when freshly applied paint fails to flow out and level. A paint maker describes it as poor flow, texture; an automotive paint source calls it poor surface texture (poor spray pattern). A detailing source stresses that orange peel is not the same as scratches, oxidation or water spots but a texture issue in the paint film itself: the surface may look shiny but not crisp. That difference decides how you fix it.

A superyacht-paint source says the closer the range between the surface and the observer the greater the visual impact of orange peel; so it stands out more on glossy, dark surfaces viewed close up. Light orange peel is common even on some factory finishes and is often accepted; heavy orange peel is a clear defect. That statement draws on automotive sources; on boats the expected quality level depends on agreement between you and the applicator.

Causes of orange peel
Figure 1. Material, technique and environment.

2. Causes: material, technique, environment#

A paint maker’s guide lists causes of orange peel in spraying: the gun held too far from the object, spray pressure too low (poor atomisation), paint film too thin and viscosity too high (paint too thick). Another maker’s guide lists paint that is too thick, an incorrect (fast) hardener or thinner and spraying at extremely high temperatures.

In roller application a boat-paint support page says that when paint is applied by roller the most common reason for orange peel is that too much paint was applied; another page from the same maker says the viscosity may be too high and can be remedied with the suitable thinner. An epoxy troubleshooting guide says cold substrate or cold material prevents levelling while hot substrate or material cures too fast to level. A forum user writes that trying to unify the coat and reworking it caused a lot of orange peel; that is one person’s experience but supports the common rule of not going back into wet paint.

Causes and first approach
CauseDetailFirst approach
High viscosityPaint too thickSuitable thinner per data sheet
Fast solvent or hardenerSurface dries too quicklyProduct speed suited to conditions
Low pressure, far gunPoor atomisationCorrect setup and distance
Too much paint on rollerMost common roller cause (maker)Less paint, tip
Extreme heat or coldSpoils flowWork at suitable temperature

3. Correction: wet sanding and polish#

A paint maker’s guide says minor orange peel can be corrected by polishing, while severe cases need sanding and respraying. An automotive care source says the fix has two sequential steps: first wet sanding to level the high points of the texture, then machine polishing to remove sanding marks and restore gloss; skipping or reversing the order gives poor results. A wood-finishing source also describes wet sanding with 1000-grit or finer paper kept moist with water or a lubricant such as mineral spirits, followed by compound and a buffing pad to restore shine.

Boat users’ experiences point the same way but are single and product dependent: a yacht owner describes hand wet sanding a hull starting at 320 and finishing at 600 grit, changing sanding direction by 90 degrees with each finer paper, and says 600 grit gave an almost polished surface. Another user writes that after wet sanding with a DA sander and 1000 and 1500 grit paper he got a mirror-like surface with a polishing method. Another user on the same forum says he could not remove deep orange peel without burning through the paint: total coating thickness is limited.

Path to correction
Figure 2. From diagnosis to prevention.

4. What to watch: paint thickness and product type#

Wet sanding has a cost: a paint film is a thin layer and every sanding takes thickness. So rather than trying to remove deep orange peel by sanding, sometimes sanding and applying one more coat is safer. A forum user writes that after three coats on the whole boat he did not want to recoat and wanted only wet sanding and polish, but could not remove deep orange peel without going through the paint. That is a single experience; consult the maker and your painter on thickness.

Two-part and one-part paints behave differently too: a hard two-part film is more durable but its wet sanding and polishing need different conditions; paint should not be sanded before fully cured. See the waiting times in the data sheet for sanding and polish. Along with salt, UV and oxidation a care plan that protects the film after correcting orange peel is also needed.

5. Prevention#

The core of prevention is providing conditions that support flow: thin the paint per the maker’s data sheet, choose solvent and hardener speed suited to ambient temperature, set correct pressure, tip and distance on the gun, do not overload the roller and apply thin coats. A paint maker’s guide advises spraying a test panel before application and avoiding spraying at high temperatures. In the roll and tip method tipping with a brush removes roller texture; see our article on it.

  1. Recognise the defect: is it really orange peel or a scratch, oxidation or contamination?
  2. Assess depth; try a small area.
  3. If light, wet sand starting with fine grit; then compound and polish.
  4. If deep consider sanding and recoating.
  5. Remove the cause: viscosity, speed, setup, paint amount, temperature.
  6. On later coats follow the data sheet and a test panel.
Wet-sand and polish sequence
Figure 3. From sanding to polish.

6. Common mistakes#

  • Intervening without telling orange peel from something else.
  • Loading the roller with too much paint.
  • Applying paint unthinned or with the wrong thinner.
  • Spraying in extreme heat.
  • Going back into wet paint to “fix” it.
  • Sanding deep orange peel until the paint is through.
  • Sanding before full cure.

7. Checklist#

Orange peel checklist0/7

8. Conclusion#

Orange peel is a texture defect from paint failing to flow and level; causes lie in material, technique and environment. For light cases wet sanding and polish work, deep cases need sanding and a recoat. Prevention rests on following the data sheet, correct setup and thin coats. This article is general information; the data sheet and expert opinion come first.

Frequently asked questions#

What is orange peel?

A textured look resembling orange skin, formed when the paint fails to flow out and level on the surface.

What are the most common causes?

Per sources high viscosity, fast solvent or hardener, low atomisation pressure, gun held far away and too much paint on the roller.

Can light orange peel be removed?

Paint-maker sources say light cases can be polished out, user experiences say wet sanding and compound; severe cases need a recoat.

What to watch when wet sanding?

A forum user writes of the risk of going through the paint to the lower coat when removing deep orange peel; film thickness is limited, so proceed carefully.

How is it prevented?

Thin the paint per the data sheet, choose the right solvent and hardener speed, check gun setup or roller loading and apply thin coats.

Was this guide helpful?

Guide content is for general information; in practice, the current technical data sheet of the product applies.