Paint and Coatings
Sandpaper Grit Selection in Surface Preparation
Sandpaper grit directly affects paint’s mechanical bond and the look of the finished surface. This article explains grit selection for stripping, fairing and priming, with recommendations from makers and general sources.
Short answer
Sandpaper grit is chosen by job: sources place coarse (about 40–80) for paint stripping and shaping filler, medium (100–150) for reducing scratches and fine (180–320) for preparation before primer and paint. A marine paint maker recommends 180–320 grit for one-part topside paints, 220 for sound painted fibreglass and gelcoat and working from 180 down to 220 for wood. Not skipping grits prevents marks showing in the end. For the exact grit see the paint and primer maker’s data sheet. This article is general information.
Key points
- Grit is chosen by job: coarse for stripping and shaping, medium for scratch reduction, fine before primer and paint.
- A marine paint maker mentions 180–320 grit for one-part topside paints and about 220 for fibreglass, gelcoat and sound old paint.
- On wood the maker advises starting at 180 and working to 220.
- Skipping grits does not save time and usually leaves marks.
- For the exact grit always see the paint and primer data sheet.
1. Why does grit selection matter?#
Sanding has two purposes: to level the surface and to create a fine profile for paint to grip. If the grit is too coarse deep scratches remain and can show even after the topcoat; if too fine the surface is not roughened enough and adhesion can suffer. Benjamin Moore’s general guide says coarser grit speeds up the job but can damage the surface and may need a second, finer pass. In the marine environment salt, UV and movement magnify mistakes, so grit selection matters even more in boat painting.
This article does not offer one “right” grit, because the right grit depends on the existing surface, the target paint system and the maker’s recommendation. The aim is to show reasonable ranges for different jobs and the reasons behind them.
2. Coarse, medium and fine grit#
Better Boat’s grit guide groups grit for marine work into three: coarse (about 40–80) for fast stock removal, heavy oxidation, stubborn paint or varnish and shaping filler; medium (about 100–150) for refining coarse scratches, fairing repairs and general preparation before finish sanding; fine (about 180–320) for primer, paint, fresh varnish coats and controlled gelcoat refinement. This is a shop blog’s classification; a maker’s recommendation takes precedence but it offers a common framework.
On abrasive type, according to an abrasives brand’s page aluminium oxide is a good first-stage choice for removing old paint, primer and varnish effectively, while silicon carbide on waterproof film discs suits wet sanding. That is a seller’s description and depends on the product. When sanding, the rule Sail Magazine gives is simple: do not skip grit sizes; it does not save time and often leaves sanding marks.
| Range | Typical job | Note |
|---|---|---|
| 40–80 | Paint stripping, heavy oxidation, shaping filler | Removes fast, leaves deep marks |
| 100–150 | Scratch reduction, after fairing, general prep | Removes coarse marks |
| 180–320 | Before primer, paint and varnish | Mechanical bond and smooth surface |
| 320 and above | Between coats, fine finishing | Per data sheet |
3. Recommendations by surface#
TotalBoat’s support pages recommend sanding the surface with 180–320 grit for most one-part marine topside paints so the paint gets the strongest mechanical bond and a smooth finish. For two-part paints the surface is usually faired smooth first and then an epoxy-based primer is applied. Another page recommends sanding fibreglass or gelcoat, previously painted surfaces in good condition and previously painted wooden boats with 220 grit; for wood, starting at 180 and working down to 220. For which sandpaper to use before a high-build epoxy primer it asks you to see the primer maker’s recommendation.
On fairing and filler work a forum participant writes that 80 grit is good for knocking down filler but can leave lines if left just under paint, and suggests finer grit such as 240 under primer and 320 after. That is a single person’s experience and varies by system. A maker blog post aimed at antifouling prep says to level ridges, runs and transitions with 60–80 grit and blend with around 100, to use 120 for the final pass on hard, dense coatings, and that hard epoxies, ablatives and copper-free formulas may specify a target grit or prep method, and following it matters for warranty and performance.
4. Hand and machine sanding#
Sanders and blocks affect the result independently of grit. On flat surfaces a long fairing board or hard block reduces waves; machine sanding with a soft pad leaves soft marks on curved surfaces. Sanding sponges are handy on curved areas. A too-aggressive grit on a machine can leave gelcoat thin in a short time; so starting with a fine grit on gelcoat and using coarse grit only when needed makes sense.
At each stage it is important to remove the previous grit’s scratches fully: if a coarse-grit scratch is not removed enough by the finer grit it stays visible under the paint. So, as Sail Magazine advises, progress through grit sizes in order and check the surface in light at each stage. Alternating sanding direction (for example turning the direction 90 degrees with each finer grit) is a method some users apply.
5. Why the maker’s recommendation comes first#
Many makers specify a target grit or surface profile in the data sheet or support pages. Mirka’s advice in PBO says that when varnishing, because each varnish has its own recommended final grit, always read the guidelines; in many cases start with a P180 ceramic net abrasive, work in small areas and consult the product supplier. For epoxy barriers, antifouling and high-performance polyurethanes a target profile or grit may likewise be specified; warranty terms may depend on it.
So the ranges in this article are only a general framework. After deciding what you will apply, choose grit by that product’s preparation steps; if unsure ask the maker’s technical support.
- Identify the existing surface and target paint system.
- Remove defects (runs, ridges, old-paint transitions) with coarse grit.
- Soften fairing and filler with medium grit.
- Finish with the maker’s recommended final grit (e.g. 180–320 or 220).
- Progress without skipping grits; check in light at each stage.
- Remove dust and wipe with solvent.
- Apply primer per the maker’s data sheet.
6. Common mistakes#
- Skipping grits.
- Leaving very coarse grit under primer.
- Using needlessly aggressive grit on gelcoat.
- Choosing grit without reading the maker’s data sheet.
- Not checking dust and sanding marks after sanding.
- Mixing wet and dry sandpapers.
- Overusing the same sheet.
7. Checklist#
8. Conclusion#
The right sandpaper grit determines both adhesion and surface quality. As a general framework coarse grit is for stripping and shaping, medium for scratch reduction and fine for before primer and paint; makers mention 180–320 for one-part topside paints and about 220 for fibreglass and gelcoat. Do not skip grits and always follow the paint and primer data sheet. This article is general information; the data sheet and expert opinion come first.
Frequently asked questions#
What grit before primer?
A marine paint maker recommends reaching 220 grit for sound painted fibreglass, gelcoat and wood; but the primer maker’s data sheet comes first.
What grit range for one-part paint?
The same maker recommends 180–320 grit sanding for most one-part topside paints for mechanical bond.
What grit after fairing?
General sources describe shaping with coarse grit, softening with finer grit and finishing around 220 before primer; for high-build epoxy primers see the maker’s recommendation.
Why is skipping grits a problem?
Sail Magazine says skipping grit sizes does not save time and often leaves sandpaper marks.
How is grit chosen for antifouling?
A maker blog post describes levelling ridges and runs with 60–80 and blending with around 100, but notes hard epoxies, ablatives and copper-free products may specify their own target grit.
Was this guide helpful?
Thank you! Your feedback has been saved.
Guide content is for general information; in practice, the current technical data sheet of the product applies.
Keep reading
Related guides
Boat Colour Selection and Solar Reflectance: Effect of Heat Absorption on Surfaces
A study of the effect of boat paint colour on solar reflectance and surface temperature.
2 min read Paint and CoatingsCauses and Diagnosis of Paint Blistering
A study of the sources, types and diagnostic approach to blistering on boat paints.
2 min read Paint and CoatingsNumber of Coats in Epoxy Coating Systems
A study of the effect of the number of coats in epoxy coating systems on protective performance and thickness.
2 min read